Minera Yanacocha Gold Mine, Peru
Since the Carachugo ore is porous, run-of-mine ore can be heap-leached without crushing. The initial heap was cyanide leached at a rate of 10 litres/h/m
2 into a 16,000m
3 pond and the solution treated in a Merrill Crowe plant.